Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | BS2782620A | 1.48 g/cm³ |
hardness | Test Condition | Test Method | Test Result |
---|
| Shore A | | 90 |
flammability | Test Condition | Test Method | Test Result |
---|
smoke | | | 75 % |
Limiting Oxygen Index | | ISO4589-2 | 32 % |
Corrosive gases in flue gas - pH | | EN50267-2-3 | 5.80 |
Supplementary Information | Test Condition | Test Method | Test Result |
---|
HalogenAcidGasEvolution | | IEC60754-1 | <0.50 % |
tear strength | | BS6469 | 8 N/mm |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile stress | | IEC60811-1-1 | 15.5 MPa |
Tensile strain | Break | IEC60811-1-1 | 170 % |
Tensile strain | | IEC60811-1-4 | 60 % |
aging | Test Condition | Test Method | Test Result |
---|
Change rate of tensile strength | | IEC60811-1-2 | -15 % |
Change rate of tensile strength | | IEC60811-1-2 | -10 % |
Changes in tensile stress during fracture | | IEC60811-1-2 | 15 % |
Changes in tensile stress during fracture | | IEC60811-1-2 | 15 % |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Conductivity of gases | | EN50267-2-3 | 2.10 µS/cm |
Thermal performance | Test Condition | Test Method | Test Result |
---|
deformation | | IEC60811-3-1 | 25 % |
deformation | | IEC60811-3-1 | 30 % |
cold shock | | IEC60811-1-4 | pass |
Cold bend | | IEC60811-1-4 | pass |
Heat-resistant stress crack | | 内部方法 | pass |
| | ISO4589-3 | 270 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.