PLA REVODE190

39
  • Properties:
    High melting point
  • Usages:
    Extrusion blow molding
    Spinning
    High end modified base material

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
density内部方法1.20 - 1.30 g/cm³
melt mass-flow rate内部方法2.0 to 10 g/10min
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strength 内部方法> 50.0 Mpa
Tensile strain内部方法> 3.0 %
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gap内部方法3.0 to 5.0 kJ/m²
Thermal performanceTest ConditionTest MethodTest Result
Glass Transition Temperature内部方法60.0 to 63.0 °C
melting temperature内部方法170 to 180 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.