Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 12 | kJ/m² |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 50 | kJ/m² |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| Hot filament ignition temperature | 1.0mm | IEC 60695-2-13 | 750 | °C |
| Burning wire flammability index | 1.0mm | IEC 60695-2-12 | 960 | °C |
| UL flame retardant rating | 1.6mm | UL 94 | V-0 | |
| 0.8mm | UL 94 | V-0 | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile strain | Break | ISO 527-2/50 | 3.0 | % |
| tensile strength | Break | ISO 527-2/50 | 90.0 | MPa |
| Tensile modulus | ISO 527-2/1 | 9000 | MPa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Ball Pressure Test | 130°C | IEC 60335-1 | Pass | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 150 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Shrinkage rate | Internal Method | 0.50 | % | |
| density | ISO 1183 | 1.43 | g/cm³ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.