Phenolic Resinoid 2277

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTMD792A,ISO11831.41 g/cm³
Shrinkage rateASTMD9550.20 %
Shrinkage rateISO294-40.20 %
Water absorption rateASTMD570,ISO620.80 %
flammabilityTest ConditionTest MethodTest Result
UL flame retardant ratingUL94V-0
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strengthYieldASTMD638,ISO527-241.4 MPa
Flexural modulusASTMD790,ISO1788960 MPa
bending strengthASTMD790,ISO17890.3 MPa
compressive strengthASTMD695,ISO604153 MPa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTMD256A110 J/m
Impact strength of cantilever beam gapISO180/2A6.8 kJ/m²
Electrical performanceTest ConditionTest MethodTest Result
dielectric strengthASTMD149,IEC60243-113 kV/mm
arc resistanceASTMD495125 sec
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.