TSU InnoTuf® HP-2150D

0

Technical Data Sheet

thermosettingTest ConditionTest MethodTest Result
Demold Time240到360 min
Resin按重量计算的混合比:100按容量计算的混合比:100
Hardener按重量计算的混合比:22按容量计算的混合比:20
Uncured PropertiesTest ConditionTest MethodTest Result
0.60 Pa·s
3.3 Pa·s
1.7E+02 hr
15到25 min
7.1 Pa·s
Cured PropertiesTest ConditionTest MethodTest Result
Supporting hardnessASTMD224045到55
tensile strengthASTMD63829.8 MPa
elongationBreakASTMD638280 %
tear strengthASTMD62473.6 kN/m
physical property Test ConditionTest MethodTest Result
densityBase Resin1.08 g/cm³
density1.09 g/cm³
density1.18 g/cm³
Shrinkage rateASTMD25660.40到0.80 %
Mechanical propertiesTest ConditionTest MethodTest Result
ASTMD406031.0 mg
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.