PP Teldene® H03ML National Petrochemical Industries Company (NATPET)

0

Technical Data Sheet

impact performanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gap23°CISO 1805.1 kJ/m²
mechanical propertiesTest ConditionTest MethodTest Result
Tensile strainBreakISO 527-2/50>50 %
Bending modulusISO 1781470 MPa
Tensile modulusISO 527-2/11500 MPa
tensile strengthYieldISO 527-2/5034.0 MPa
tensile strengthBreakISO 527-2/5023.0 MPa
Tensile strainYieldISO 527-2/5012 %
thermal performanceTest ConditionTest MethodTest Result
Hot deformation temperature0.45MPa,UnannealedISO 75-2/B85.0 °C
Vicat softening temperatureISO 306/A50154 °C
Physical propertiesTest ConditionTest MethodTest Result
density23°CISO 11830.900 g/cm³
melt mass-flow rate230°C/2.16kgASTM D12383.2 g/10min
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.