Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | GB/T1033 | 1.20 g/cm³ |
flammability | Test Condition | Test Method | Test Result |
---|
UL flame retardant rating | | UL 94 | V-0 |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Charpy Notched Impact Strength | | GB/T1043 | 15 kJ/m² |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | | GB/T1040 | 125 MPa |
Tensile strain | Break | GB/T1040 | 10 % |
bending strength | | GB/T1042 | 200 MPa |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Volume resistivity | | GB/T1410 | 1E+15 ohms·cm |
dielectric strength | | GB/T1408 | 18 kV/mm |
dielectric constant | | GB/T1409 | 3.00 |
Dissipation Factor | | GB/T1409 | 1E-03 |
Surface Resistivity | | GB/T1410 | 1E+16 ohms |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Hot deformation temperature (HDT) | | GB/T1634 | 150 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.