plas
Log In

PP Homopolymer Polypropylene PPC100NA/2I-20M NAT Chase Plastics Services Inc.

0

Technical Data Sheet

impact performanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTM D2561100 J/m
Impact strength of cantilever beam gap23°CASTM D256110 J/m
mechanical propertiesTest ConditionTest MethodTest Result
Bending modulusASTM D7901000to1140 MPa
elongationYieldASTM D63810 %
tensile strengthYieldASTM D63821.0 MPa
thermal performanceTest ConditionTest MethodTest Result
Hot deformation temperature1.8MPa,UnannealedASTM D64850.0 °C
Hot deformation temperature0.45MPa,UnannealedASTM D64890.0 °C
Physical propertiesTest ConditionTest MethodTest Result
melt mass-flow rate190°C/2.16kgASTM D123820 g/10min
densityASTM D7920.902 g/cm³
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.