Technical Data Sheet
物理性能 | Test Condition | Test Method | Test Result |
---|---|---|---|
密度 | ASTMD792 | 0.940 g/cm³ | |
熔体质量流动速率 | 190°C/2.16kg | ASTMD1238 | 1.3 g/10min |
离子类型 | 钠(Na |
薄膜 | Test Condition | Test Method | Test Result |
---|---|---|---|
薄膜厚度-经测试 | 51 µm | ||
抗张强度 | MD:屈服,51µm | ASTMD882 | 15.2 MPa |
TD:屈服,51µm | ASTMD882 | 12.5 MPa | |
MD:断裂,51µm | ASTMD882 | 33.6 MPa | |
TD:断裂,51µm | ASTMD882 | 34.3 MPa | |
伸长率 | MD:断裂,51µm | ASTMD882 | 280 % |
TD:断裂,51µm | ASTMD882 | 400 % |
热性能 | Test Condition | Test Method | Test Result |
---|---|---|---|
溶融温度 | 内部方法 | 95.0 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.