physical propertyTest ConditionTest MethodTest ResultUnit
densityASTM D-7920.959g/cm
Melt mass flow rate190℃/2.16kgASTM D-12388g/10min
Mechanical performanceTest ConditionTest MethodTest ResultUnit
Environmental stress cracking50℃,2mm,100% Igepal,Compression Molded,F50ASTM D-1693B5hr
Shore hardnessShore D,15 sec,Compression MoldedASTM D-224063
Tensile yield strengthCompression MoldedASTM D-63829Mpa
Tensile yield elongationCompression MoldedASTM D-6387.5%
Bending modulus -2% SecantCompression MoldedASTM D-7901140Mpa
Impact strength of cantilever beam gapCompression MoldedASTM D-25635J/m
Thermal performanceTest ConditionTest MethodTest ResultUnit
Hot deformation temperature0.45MPa, Unannealed,Compression MoldedASTM D-64876°C
vicat softening pointASTM D-1525126°C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.