PA6 B3ZG3 BASF GERMANY
50
Form:Granules | Grade:Impact resistant grade
Properties:
Dimensional stabilityGlass fiber reinforcedFiller: Glass fiber reinf15% filler by weight
Typical Applications:
sporting goodscatheterApplication in the automotive field
Product Description
Certificates(1)
Datasheet
Alternative Model(2)
Product Description
| Typical Applications: | sporting goods | catheter | Application in the automotive field |
| Properties: | Dimensional stability | Glass fiber reinforced | Filler: Glass fiber reinf | 15% filler by weight |
Certificates

Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Charpy Notched Impact Strength | -30°C | ISO 179 | 4.0 | kJ/m² |
| 23°C | ISO 179 | 12 | kJ/m² | |
| Impact strength of cantilever beam gap | -30°C | ISO 180 | 4.0 | kJ/m² |
| 23°C | ISO 180 | 12 | kJ/m² | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile modulus | 23°C | ISO 527-2 | 5300 | Mpa |
| tensile strength | Break,23°C | ISO 527-2 | 100 | Mpa |
| Tensile strain | Break,23°C | ISO 527-2 | 3.8 | % |
| Bending modulus | 23°C | ISO 178 | 4500 | Mpa |
| bending strength | 23°C | ISO 178 | 150 | Mpa |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 190 | °C |
| Melting temperature | ISO 3146 | 220 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ISO 1183 | 1.22 | g/cm³ | |
| Water absorption rate | Saturation,23°C | ISO 62 | 7.5 | % |
| Equilibrium,23°C,50%RH | ISO 62 | 2.4 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.