PUR-Ester Witcobond® W-242 CHEMTURU USA
Product Description
Certificates(0)
Datasheet
Product Description
Certificates
No Data...
Technical Data Sheet
| elastomer | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| tensile strength | 53.8 | MPa | ||
| elongation | Break | 50 | % | |
| thermosetting | Test Condition | Test Method | Test Result | Test Unit |
| Thermosetting mixed viscosity | 25°C | <600 | cP | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Glass transition temperature | 1.00 | °C | ||
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | 1.05 | g/cm³ | ||
| PH value | 25°C | 7.2to9.2 | ||
| Solid content | 34to36 | % | ||
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Pencil hardness | 2H | |||
| Shore hardness | 52.0 | |||
| Supplementary Information | Test Condition | Test Method | Test Result | Test Unit |
| MinimumFilm Forming | 0 | °C | ||
| Cosolvent-N-Methylpyrrolidone | 7.3 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.