TPE 4001 USA Nova
0
- Properties:Good coloring and chemical resistance
Technical Data Sheet
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Permanent compression deformation | 100℃,22hr | ASTM D-395 | 41 % |
| 70℃,22hr | ASTM D-395 | 34 % | |
| 25℃,22hr | ASTM D-395 | 20 % | |
| tear strength | ASTM D-624 | 20.5 kN/m | |
| elongation | Break | ASTM D-412 | 280 % |
| tensile strength | Break | ASTM D-412 | 3.55 MPa |
| Shore hardness | 15sec | ASTM D-2240 | 45 |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Brittle temperature | ASTM D-746 | -40 ℃ |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| density | ASTM D-792 | 0.949 g/cm3 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.