| Typical Applications: | Electronic and electrical components | Automotive Applications |
| Properties: | Thermal stability | Filler: Glass fiber reinf | Filler by weight |
Certificates

Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 18 | kJ/m² |
| -30°C | ISO 180/1A | 15 | kJ/m² | |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 120 | kJ/m² |
| -30°C | ISO 179/1eU | 120 | kJ/m² | |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 20 | kJ/m² |
| -30°C | ISO 179/1eA | 19 | kJ/m² | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| FMVSS flammability | FMVSS302 | B | ||
| Flammability level | 1.5mm | IEC 60695-11-10,-20 | HB | |
| UL flame retardant rating | 1.5mm | UL 94 | HB | |
| Burning rate | 1.00mm | ISO 3795 | 44 | mm/min |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile modulus | ISO 527-2 | 14500 | Mpa | |
| tensile strength | Break | ISO 527-2 | 230 | Mpa |
| Tensile strain | Break | ISO 527-2 | 3.0 | % |
| Bending modulus | ISO 178 | 13000 | Mpa | |
| Tensile creep modulus | 1000hr | ISO 899-1 | -- | Mpa |
| 1hr | ISO 899-1 | -- | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Vicat softening temperature | ISO 306/B50 | 215 | °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 213 | °C |
| 0.45MPa,Unannealed | ISO 75-2/B | 221 | °C | |
| Linear coefficient of thermal expansion | TD | ISO 11359-2 | 1E-04 | cm/cm/°C |
| MD | ISO 11359-2 | 1.6E-05 | cm/cm/°C | |
| Melting temperature | ISO 11357-3 | 221 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | Equilibrium,23°C,2.00mm,50%RH | ISO 62 | 1.5 | % |
| Saturation,23°C,2.00mm | ISO 62 | 4.9 | % | |
| Shrinkage rate | MD | ISO 294-4 | 0.10 | % |
| TD | ISO 294-4 | 0.90 | % | |
| density | ISO 1183 | 1.51 | g/cm³ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.