AS 300V
0
- Properties:Antistatic functioncopolymergood chemical resistanceand good processing performance
- Usages:Audio tapesautomotive applicationselectricalelectronic applicationsvideo tapes
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTM D-792 | 1.07 g/cm | |
Shrinkage rate | ASTM D-955 | 0.20-0.60 % |
Basic performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Water absorption rate | ASTM D-570 | 0.030 % | |
melt mass-flow rate | ASTM D-1238 | 25 g/10min |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | ASTM D-638 | 73.4 MPa | |
elongation at yield | ASTM D-638 | 4.0 % | |
Flexural modulus | ASTM D-790 | 3430 MPa | |
bending strength | ASTM D-790 | 88.1 MPa | |
Impact strength of cantilever beam gap | ASTM D-256 | 14.9 J/m | |
Rockwell hardness | ASTM D-785 | 87 M scale |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Volume resistivity | ASTM D-257 | 1E+12 ohm.cm | |
dielectric strength | ASTM D-149 | 21.7 KV/mm | |
dielectric constant | ASTM D-150 | 2.500 |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat distortion temperature | ASTM D-648 | 92.2 ℃ | |
vicat | ASTM D-1525 | 105 ℃ | |
combustibility | UL 94 | HB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.
Contact Us
Get App
Top