| elastomer | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| tensile strength | 100%Strain | ASTMD412 | 13.0 | Mpa |
| 300%Strain | ASTMD412 | 25.0 | Mpa | |
| Yield | ASTMD412 | 47.0 | Mpa | |
| elongation | Break | ASTMD412 | 480 | % |
| tear strength | --1 | ASTM D624 | 169 | kN/m |
| --2 | ISO 34-1 | 170 | kN/m | |
| Permanent compression deformation | 23°C,70hr | ASTM D395B | 18 | % |
| 70°C,22hr | ASTM D395B | 23 | % | |
| 100°C,70hr | ASTM D395B | 36 | % | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Wear amount | ISO 4649 | 29.0 | mm³ | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Glass transition temperature | ISO 11357-2 | -38.0 | °C | |
| Melting temperature | Internal Method | 215to225 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| water content | Internal Method | <0.10 | % | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Shore hardness | ShoreD | ASTMD2240 | 45 | |
| ShoreA | ASTMD2240 | 94 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.