TPU ESTANE® T470A-3 LUBRIZOL SHANGHAI
27
- Properties:Low hardness
Technical Data Sheet
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Permanent compression deformation | 23℃,22.0hr | ASTM D-395 | 10 % |
| tear strength | ASTM D-624 | 73.5 kN/m | |
| elongation | Break | 900 % | |
| tensile strength | Yield | 27.5 MPa | |
| 300%Strain | MPa | ||
| 100%Strain | ASTM D-412 | 3.53 Mpa |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Vicat softening temperature | ASTM D-1525 | 77 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Shore hardness | ShoreA | ASTM D-2240 | 77 |
| Shrinkage rate | MD | ASTM D-955 | 0.60 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.