PA6 HiFill® PA6 GF15 IM1

0
  • Properties:
    Filler
    glass fiber reinforced material
    15%
    filler by weight

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTMD7921.23 g/cm³
Shrinkage rateASTMD9550.30 %
Water absorption rateASTMD5700.20 %
hardnessTest ConditionTest MethodTest Result
Rockwell hardnessR-ScaleASTMD785112
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTMD256210 J/m
Impact strength of cantilever beam gapASTMD25691 J/m
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strengthBreakASTMD63889.6 MPa
elongationBreakASTMD6384.5 %
Flexural modulusASTMD7904140 MPa
bending strengthASTMD790172 MPa
Electrical performanceTest ConditionTest MethodTest Result
Volume resistivityASTMD2571E+15 ohms·cm
dielectric strengthASTMD14916 kV/mm
Thermal performanceTest ConditionTest MethodTest Result
ASTMD648193 °C
ASTMD6961.8E-05 cm/cm/°C
ASTMD648213 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.

Contact Us