Unspecified MAJORIS FFR200 BEIGE 7605 AD MAJORIS FRANCE
Product Description
Certificates(0)
Datasheet
Product Description
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | -30°C | ISO 180 | 2.0 | kJ/m² |
| Charpy Notched Impact Strength | 23°C | ISO 179 | 2.3 | kJ/m² |
| -30°C | ISO 179 | 1.4 | kJ/m² | |
| Impact strength of cantilever beam gap | 23°C | ISO 180 | 2.3 | kJ/m² |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| Extreme Oxygen Index | ISO 4589-2 | 28 | % | |
| Burning wire flammability index | 2.0mm | IEC 60695-2-12 | 960 | °C |
| UL flame retardant rating | 2.0mm | UL 94 | 5VA | |
| 3.2mm | UL 94 | V-0 | ||
| 1.6mm | UL 94 | V-0 | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Bending modulus | ISO 178 | 2650 | MPa | |
| Tensile strain | Break | ISO 527-2/50 | 7.0 | % |
| Yield | ISO 527-2/50 | 3.0 | % | |
| tensile strength | Break | ISO 527-2/50 | 26.0 | MPa |
| Yield | ISO 527-2/50 | 27.0 | MPa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Vicat softening temperature | ISO 306/A | 142 | °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 71.0 | °C |
| 0.45MPa,Unannealed | ISO 75-2/B | 127 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 16 | g/10min |
| density | ISO 1183 | 1.36 | g/cm³ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.