Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Shrinkage rate | | ASTMD955 | 0.10到0.20 % |
Water absorption rate | | ASTMD570 | 0.070 % |
density | | ASTMD792 | 1.84 g/cm³ |
hardness | Test Condition | Test Method | Test Result |
---|
Barcol Hardness | | ASTMD2583 | 30 |
flammability | Test Condition | Test Method | Test Result |
---|
UL flame retardant rating | | UL94 | V-0 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | Yield | ASTMD638 | 20.7 MPa |
Flexural modulus | | ASTMD790 | 6890 MPa |
bending strength | Yield | ASTMD790 | 68.9 MPa |
compressive strength | | ASTMD695 | 110 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of cantilever beam gap | | ASTMD256 | 53 J/m |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Volume resistivity | | ASTMD257 | 1.5E+14 ohms·cm |
dielectric strength | | ASTMD149 | 16 kV/mm |
arc resistance | | ASTMD495 | 180 sec |
Compared to the Leakage Tracking Index (CTI) | | UL746 | 500 V |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTMD648 | 204 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.