Share
Add to compare

PP Homopolymer HIPOLEN P® MN 1TS Hipol a.d.

Product Description
Certificates(0)
Datasheet

Product Description

Certificates

No Data...

Technical Data Sheet

impact performanceTest ConditionTest MethodTest ResultTest Unit
Impact strength of cantilever beam gap23°CISO 1803.1kJ/m²
mechanical propertiesTest ConditionTest MethodTest ResultTest Unit
Tensile modulusISO 527-21650MPa
Bending modulusISO 1781600MPa
tensile strengthYieldISO 527-237.0MPa
thermal performanceTest ConditionTest MethodTest ResultTest Unit
Vicat softening temperatureISO 306/A50155°C
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
melt mass-flow rate230°C/2.16kgISO 113342g/10min
densityISO 1183/D0.910g/cm³
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.