DAP Generic DAP - Mineral

0
  • Properties:
    Filler
    mineral filler

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTM D7921.75to1.86 g/cm³
Shrinkage rateASTM D18952.3
Shrinkage rateASTM D9550.25to0.51 %
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strength ASTM D63851.7to55.2 MPa
Flexural modulusASTM D7908170to11700 MPa
bending strengthASTM D79089.6to104 MPa
compressive strengthASTM D695144to152 MPa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTM D25621to32 J/m
Electrical performanceTest ConditionTest MethodTest Result
dielectric strengthASTM D14914to16 kV/mm
dielectric constantASTM D1503.68to4.70
Dissipation FactorASTM D1500.010to0.025
arc resistanceASTM D495135to180 sec
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureASTM D648161to274 °C
Linear coefficient of thermal expansionASTM D6962.5E-5到4.6E-5 cm/cm/°C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.