HIPS GH660 Guangzhou Petrochemical
Properties:
Characteristics with high impact resistance and good processing properties
Typical Applications:
Suitable for high impact injection molding widely used in various parts such as mechanical components toys and home appliance casings
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Suitable for high impact injection molding | widely used in various parts such as mechanical components | toys | and home appliance casings |
| Properties: | Characteristics | with high impact resistance and good processing properties |
Certificates
No Data...
Technical Data Sheet
| Other performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| styrene content | GB/T 4614 | 合格|≤800 | mg/kg | |
| GB/T 4614 | 一级|≤800 | mg/kg | ||
| GB/T 4614 | 优级|≤800 | mg/kg | ||
| Particle size distribution | 污染粒子 | SH/T 1541 | 合格|≤15 | 个/kg |
| 污染粒子 | SH/T 1541 | 一级|≤15 | 个/kg | |
| 污染粒子 | SH/T 1541 | 优级|≤7 | 个/kg | |
| Basic Performance | Test Condition | Test Method | Test Result | Test Unit |
| melt mass-flow rate | GB/T 3682 | 合格|4.5-7.5 | g/10min | |
| GB/T 3682 | 一级|4.5-7.5 | g/10min | ||
| GB/T 3682 | 优级|4.5-7.5 | g/10min | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| tensile strength | Yield | GB/T 1040 | 合格|≥18 | MPa |
| Yield | GB/T 1040 | 一级|≥18 | MPa | |
| Yield | GB/T 1040 | 优级|≥18 | MPa | |
| elongation | GB/T 1040 | 合格|≥30 | % | |
| GB/T 1040 | 一级|≥30 | % | ||
| GB/T 1040 | 优级|≥30 | % | ||
| Impact strength of cantilever beam gap | GB/T 1843 | 合格|≥30 | J/m | |
| GB/T 1843 | 一级|≥30 | J/m | ||
| GB/T 1843 | 优级|≥30 | J/m | ||
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Vicat softening temperature | GB/T 1633 | 合格|≥87 | ℃ | |
| GB/T 1633 | 一级|≥87 | ℃ | ||
| GB/T 1633 | 优级|≥87 | ℃ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.