TPU-Ester 770 A 15 CS 000 BASF GERMANY

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityISO 1183/A1.15 g/cm³
hardnessTest ConditionTest MethodTest Result
Shore hardnessISO 761970
Mechanical propertiesTest ConditionTest MethodTest Result
Wear amountISO 4649-A50.0 mm³
elastomerTest ConditionTest MethodTest Result
tensile strength YieldDIN 53504-S227.0 MPa
elongationBreakDIN 53504-S2650 %
tear strengthISO 34-145 kN/m
compression setISO 81523 %
compression setISO 81527 %
compression setISO 81545 %
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.