other | Test Condition | Test Method | Test Result |
---|
characteristic | | | V2, |
colour | | | 清淅透明,浅蓝底 |
purpose | | | 薄壁制品,手机配件,家电配件 |
optical performance | Test Condition | Test Method | Test Result |
---|
transmittance | | ASTM D1003/ISO 13468 | 89% % |
processability | Test Condition | Test Method | Test Result |
---|
Dry conditions | | | 120度 五小时 |
Temperature | | | 70-90 °C |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Charpy impact strength | | ASTM D256/ISO 179 | 69 kg·cm/cm(J/M)ft·lb/in |
elongation at break | | ASTM D638/ISO 527 | 119 % |
Tensile modulus | | ASTM D638/ISO 527 | 2400 kg/cm²(MPa)[Lb/in²] |
Flexural modulus | | ASTM D790/ISO 178 | 2300 kg/cm²(MPa)[Lb/in²] |
bending strength | | ASTM D790/ISO 178 | 93 kg/cm²(MPa)[Lb/in²] |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Surface Resistivity | | ASTM D257/IEC 60093 | 6E+15 Ω |
dielectric constant | | ASTM D150/IEC 60250 | 3.1 |
Volume resistivity | | ASTM D257/IEC 60093 | 3E+14 Ω.cm |
Physical properties | Test Condition | Test Method | Test Result |
---|
density | | ASTM D792/ISO 1183 | 1.2 |
Mold Shrinkage | | ASTM D955 | 0.5-0.7 % |
melt mass-flow rate | | ASTM D1238/ISO 1133 | 16 g/10min |
Water absorption rate | | ASTM D570/ISO 62 | 0.24 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.