Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | GB/T 1033 | 1200 kg/m3 |
Shrinkage rate | | GB/T 39818 | 0.6-0.8 % |
average molecular weight | | GB/T 36214 | 20500 g/mol |
Number of impurity particles | | 内部测试方法 | 0.0 个/kg |
melt mass-flow rate | | GB/T 3682 | 10 g/10min |
optical performance | Test Condition | Test Method | Test Result |
---|
transmittance | | GB/T 2410 | 89 % |
Yellowness Index | | GB/T 39822 | 0.0-1 YI |
Color | | GB/T 39822 | 0.1-0.5 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | | GB/T 1040 | 60 Mpa |
elongation at break | | GB/T 1040 | 105 % |
bending strength | | GB/T 9341 | 95 Mpa |
Charpy Notched Impact Strength | | GB/T 1043 | 65 KJ/m 2 |
Flame retardant performance | Test Condition | Test Method | Test Result |
---|
UL flame retardant rating | | UL 94 | V-2 |
Limiting Oxygen Index | | GB/T 2406 | 27 % |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Heat distortion temperature | | GB/T 1634 | 123 ℃ |
vicat | | GB/T 1633 | 140 ℃ |
Glass Transition Temperature | | GB/T 19466 | 147 ℃ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.