Test Condition | Test Method | Test Result | |
---|---|---|---|
熔融峰值温度 | ASTMD3417 | 85.0 °C | |
AllowableCoatingSpeed | 250°C | >5.0 m/sec | |
始封温度 | 80.0 °C | ||
脆化温度 | ASTMD746 | <-76.0 °C | |
维卡软化温度 | ASTMD1525 | 61.0 °C | |
密度 | ASTMD1505 | 0.939 g/cm³ | |
熔体质量流动速率 | 190°C/2.16kg | ASTMD1238 | 16 g/10min |
醋酸乙烯含量 | 内部方法 | 18.0 wt% | |
抗张强度 | Break | ASTMD638 | 13.5 MPa |
伸长率 | Break | ASTMD638 | 860 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.