PPS R-4-230NA CPCHEM USA
225
Form:Granules | Grade:Extrusion grade
Properties:
Easy to processFiller: Glass fiber reinf40%Filler by weight
Typical Applications:
Electrical applicationsElectrical/Electronic Applications
Product Description
Certificates(1)
Datasheet
Product Description
| Typical Applications: | Electrical applications | Electrical/Electronic Applications |
| Properties: | Easy to process | Filler: Glass fiber reinf | 40% | Filler by weight |
Certificates

Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | 3.17mm | ASTM D256 | 91 | J/m |
| ISO 180/A | 9.0 | kJ/m² | ||
| Suspended wall beam without notch impact strength | 3.18mm | ASTM D4812 | 450 | J/m |
| ISO 180 | 25 | kJ/m² | ||
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 1.6mm | UL 94 | V-05VA | |
| Extreme Oxygen Index | ASTM D2863 | 50 | % | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Poisson's ratio | 0.43 | |||
| compressive strength | ASTM D695 | 275 | Mpa | |
| bending strength | ISO 178 | 245 | Mpa | |
| ASTM D790 | 228 | Mpa | ||
| Bending modulus | ISO 178 | 14000 | Mpa | |
| ASTM D790 | 14500 | Mpa | ||
| Tensile strain | Break | ISO 527-2 | 1.3 | % |
| elongation | Break | ASTM D638 | 1.2 | % |
| tensile strength | ISO 527-2 | 170 | Mpa | |
| ASTM D638 | 179 | Mpa | ||
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| UL temperature rating | UL 746B | 200to220 | °C | |
| Linear coefficient of thermal expansion | TD:导热系数 | ASTME831 | 0.31 | W/m/K |
| TD:100to200°C | ASTME831 | 8E-05 | cm/cm/°C | |
| TD:-50to50°C | ASTME831 | 4E-05 | cm/cm/°C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ASTM D648 | 265 | °C |
| Linear coefficient of thermal expansion | MD:-50to50°C | ASTME831 | 1.5E-05 | cm/cm/°C |
| MD:100to200°C | ASTME831 | 1.5E-05 | cm/cm/°C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Shrinkage rate | TD:3.20mm | 0.50 | % | |
| MD:3.20mm | 0.20 | % | ||
| density | ASTM D792 | 1.68 | g/cm³ | |
| Water absorption rate | 23°C,24hr | ASTM D570 | 0.020 | % |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dissipation factor | 25°C,1kHz | ASTM D150 | 2E-03 | |
| Dielectric constant | 25°C,1MHz | ASTM D150 | 3.90 | |
| 25°C,1kHz | ASTM D150 | 3.90 | ||
| Dielectric strength | ASTM D149 | 20 | KV/mm | |
| Volume resistivity | ASTM D257 | 1E+16 | ohms·cm | |
| Surface resistivity | ASTM D257 | 1E+16 | ohms | |
| Dissipation factor | 25°C,1MHz | ASTM D150 | 2E-03 | |
| Arc resistance | ASTM D495 | 125 | sec | |
| Compared to the anti leakage trace index | CTI | UL 746 | PLC 4 | |
| insulation resistance | 90°C | 1E+12 | ohms | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | M-Sale | ASTM D785 | 104 | |
| R-Sale | ASTM D785 | 122 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.