PUR-Ester Witcobond® A-100 CHEMTURU USA

0

Technical Data Sheet

thermosettingTest ConditionTest MethodTest Result
Thermosetting mixed viscosity5.00to100 cP
physical property Test ConditionTest MethodTest Result
density1.05 g/cm³
pH value7.0to9.0
Solid Content34to36 %
hardnessTest ConditionTest MethodTest Result
Hardness3H
Shore hardness64.0
elastomerTest ConditionTest MethodTest Result
tensile strength 44.8 MPa
tensile strength 49.6 MPa
elongationBreak140 %
Thermal performanceTest ConditionTest MethodTest Result
Glass Transition Temperature77.0 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.