PA66 Staramide AK8 EUROSTAR FRANCE
Properties:
Filler mineral filler 40% filler by weight
Product Description
Certificates(0)
Datasheet
Product Description
| Properties: | Filler | mineral filler | 40% | filler by weight |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Charpy Notched Impact Strength | -30°C | ISO 179/1eA | 6.0 | kJ/m² |
| 23°C | ISO 179/1eA | 7.0 | kJ/m² | |
| Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | >100 | kJ/m² |
| 23°C | ISO 179/1eU | >100 | kJ/m² | |
| Impact strength of cantilever beam gap | -30°C | ISO 180/1A | 7.0 | kJ/m² |
| 23°C | ISO 180/1A | 7.0 | kJ/m² | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| Burning wire flammability index | 2.0mm | IEC 60695-2-12 | 650 | °C |
| Extreme Oxygen Index | ISO 4589-2 | 32 | % | |
| Burning rate | 2.00mm | FMVSS302 | 6.0 | mm/min |
| 3.00mm | FMVSS302 | 2.0 | mm/min | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile modulus | ISO 527-2/1 | 5200 | MPa | |
| tensile strength | Break | ISO 527-2/5 | 75.0 | MPa |
| Tensile strain | Break | ISO 527-2/5 | 10 | % |
| Bending modulus | ISO 178 | 5200 | MPa | |
| bending strength | ISO 178 | 135 | MPa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | MD:23to60°C | ISO 11359-2 | 6E-05 | cm/cm/°C |
| TD:23to60°C | ISO 11359-2 | 6E-05 | cm/cm/°C | |
| Hot deformation temperature | 0.45MPa,Unannealed,100mmSpan | ISO 75-2/Be | 231 | °C |
| 1.8MPa,Unannealed,100mmSpan | ISO 75-2/Ae | 170 | °C | |
| Vicat softening temperature | -- | ISO 306/B50 | 252 | °C |
| -- | ISO 306/B120 | 251 | °C | |
| Ball Pressure Test | 125°C | IEC 60695-10-2 | 通过 | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ISO 1183 | 1.45 | g/cm³ | |
| Shrinkage rate | MD | Internal Method | 0.90to1.3 | % |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.90 | % |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dielectric strength | 3.20mm,in Oil | IEC 60243-1 | 18 | kV/mm |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | L-Sale | ISO 2039-2 | 92 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.