physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
Shrinkage rate | ISO294-4 | 0.20to0.60 % | |
Water absorption rate | ASTMD570 | 0.10 % | |
ISO62 | 0.10 % | ||
density | ASTMD792 | 1.04 g/cm³ | |
ISO1183 | 1.04 g/cm³ | ||
melt mass-flow rate | ASTMD1238 | 3.5 g/10min | |
Melt volume flow rate | ISO1133 | 3.50 cm3/10min | |
Shrinkage rate | ASTMD955 | 0.20to0.60 % |
optical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Haze ratio | ASTMD1003 | 2.0 % | |
refractive index | ASTMD542 | 1.570 | |
ISO489 | 1.570 | ||
transmissivity | ASTMD1003 | 90.0 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile modulus | ASTMD638 | 2240 Mpa | |
ISO527-2 | 2240 Mpa | ||
tensile strength | ASTMD638 | 27.6 Mpa | |
Tensile stress | ISO527-2 | 28.0 Mpa | |
elongation | ASTMD638 | 40 % | |
Flexural modulus | ASTMD790 | 2280 Mpa | |
ISO178 | 2280 Mpa | ||
bending strength | ASTMD790 | 55.2 Mpa | |
Bending stress | ISO178 | 55.0 Mpa | |
Rockwell hardness | ASTMD785 | 80 |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat Deflection Temperature | 92.2 °C | ||
vicat | ASTMD15253 | 97.8 °C | |
maximum service temperature | 250 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.