PP F327BV PRIME POLYMER JAPAN
54
Form:Granules | Grade:Thin film grade
Typical Applications:
film
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | film |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of simply supported beam without notch | 23°C | ISO 179 | 12 | kJ/m² |
| Basic Performance | Test Condition | Test Method | Test Result | Test Unit |
| melt mass-flow rate | 230℃ | ISO 1133 | 7 | g/10min |
| density | ISO 1183 | 0.910 | g/cm³ | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Load resistant bending temperature | ISO 75 | 80 | °C | |
| Shore hardness | R-Scale | ISO 2039-2 | 85 | |
| tensile strength | ISO 527 | 23 | Mpa | |
| elongation | ISO 527 | 200 | ||
| Impact strength of cantilever beam gap | 23℃ | ISO 179 | 12 | kJ/m² |
| Tensile modulus | ISO 527-2 | 850 | Mpa | |
| tensile strength | Yield | ISO 527-2 | 23.0 | Mpa |
| Tensile strain | Break | ISO 527-2 | >200 | % |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 80.0 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 7.0 | g/10min |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | R-Sale | ISO 2039-2 | 85 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.