Technical Data Sheet
thermosetting | Test Condition | Test Method | Test Result |
---|
Thermosetting components | Resin | | 按容量计算的混合比:2.8按重量计算的混合比:100 |
Thermosetting components | Hardener | | 按容量计算的混合比:1.0按重量计算的混合比:20 |
Thermosetting components | | | 140to180 min |
Thermosetting components | | | 52 wk |
Thermosetting mixed viscosity | | ASTM D2393 | 5500 cP |
stripping time | | | 7200to10000 min |
physical property | Test Condition | Test Method | Test Result |
---|
Apparent density | | ASTM D1895 | 1.44 g/cm³ |
Shrinkage rate | | ASTM D955 | 0.050 % |
hardness | Test Condition | Test Method | Test Result |
---|
Shore hardness | | ASTM D2240 | 89 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
compressive strength | | ASTM D695 | 79.2 MPa |
Tensile modulus | | ASTM D638 | 4900 MPa |
tensile strength | Break | ASTM D638 | 38.6 MPa |
elongation | Yield | ASTM D638 | 0.90 % |
Flexural modulus | | ASTM D790 | 3720 MPa |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Linear coefficient of thermal expansion | | ASTM D696 | 5.7E-05 cm/cm/°C |
Heat distortion temperature | | ASTM D648 | 65.6 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.