Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Water absorption rate | | GB/T1034 | 0.50 % |
ash content | | GB/T9345 | 0.15 % |
density | | GB/T1033 | 1.34to1.36 g/cm³ |
melt mass-flow rate | | GB/T3682 | 25to700 g/10min |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | | GB/T1040 | 100 MPa |
Tensile strain | Break | GB/T1040 | 30 % |
bending strength | | GB/T1042 | 120 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Charpy Notched Impact Strength | | GB/T1043 | 18 kJ/m² |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Surface Resistivity | | GB/T1410 | 1E+13 ohms |
Volume resistivity | | GB/T1410 | 1E+12 ohms·cm |
dielectric constant | | GB/T1409 | 3.00 |
dielectric constant | | GB/T1409 | 3.00 |
Dissipation Factor | | GB/T1409 | 6E-04 |
Dissipation Factor | | GB/T1409 | 1.5E-03 |
Thermal performance | Test Condition | Test Method | Test Result |
---|
melting temperature | | GB/T4608 | 310 °C |
Hot deformation temperature (HDT) | | GB/T1634 | 110 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.