PA6 Tekumid 6 SC/GF15

0
  • Properties:
    Filler
    glass fiber reinforced material
    15%
    filler by weight

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTMD7921.25 g/cm³
Ash Content15 %
Supplementary InformationTest ConditionTest MethodTest Result
HeatResistanceASTMD648198 °C
Mechanical propertiesTest ConditionTest MethodTest Result
Flexural modulusASTMD7905000 MPa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTMD25660 J/m
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.