Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Water absorption rate | | ISO62 | 1.4 % |
density | | ISO1183 | 1.33 g/cm³ |
other | Test Condition | Test Method | Test Result |
---|
proof tracking index | | IEC60112 | 500 V |
Surface Resistivity | | IEC60093 | 1.00E+14 Ω |
Linear forming shrinkage rate | | ISO2577 | 0.8 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile strength at break | | ISO527 | 80 Mpa |
elongation at break | | ISO527 | 3.0 % |
Yield bending strength | | ISO178 | 130 Mpa |
Flexural modulus | | ISO178 | 5000 Mpa |
Charpy Notched Impact Strength | | ISO179 | 4.5 kJ/m² |
Impact strength of simply supported beam without notch | | ISO179 | 40 kJ/m² |
Flame retardant performance | Test Condition | Test Method | Test Result |
---|
Flame retardant performance UL94 | | UL94 | ℃ |
Flame retardant performance UL94 | | UL94 | V-2 ℃ |
Flame retardant performance UL94 | | UL94 | ℃ |
Flame retardant performance UL94 | | UL94 | ℃ |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Hot deformation temperature 1.8MPa | | ISO76 | 170 ℃ |
Hot deformation temperature 0.45MPa | | ISO76 | ℃ |
GWFI | | IEC60695-2-12 | 960 ℃ |
GWFI | | IEC60695-2-12 | ℃ |
GWFI | | IEC60695-2-12 | ℃ |
GWFI | | IEC60695-2-12 | ℃ |
GWIT | | IEC60695-2-13 | ℃ |
GWIT | | IEC60695-2-13 | ℃ |
GWIT | | IEC60695-2-13 | ℃ |
GWIT | | IEC60695-2-13 | ℃ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.