PETG WS-501N JIANGYIN HUAHONG
245
Form:Granules
Properties:
High toughnessHigh gloss
Typical Applications:
Electrical applications
Product Description
Certificates(1)
Datasheet
Product Description
| Typical Applications: | Electrical applications |
| Properties: | High toughness | High gloss |
Certificates

Technical Data Sheet
| optical performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| turbidity | / | < 1.0 | % | |
| Transmittance rate | ASDM D541 | 90 | % | |
| Refractive index | ASDM D542 | 1.56 | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | R-Scale | 117 | °C | |
| Izod Notched Impact Strength | 23°C | ASTM D256 | 102 | J/m |
| Dart impact | Normal temperature | ASTM D358 | 1803 | g |
| Low temperature | ASTM D358 | 829 | g | |
| Bending modulus | 1.27mm/min(3 inch/min) | ASTM D790 | 21200 | Kgf/cm2 |
| bending strength | 1.27mm/min(2 inch/min) | ASTM D790 | 680 | Kgf/cm2 |
| elongation | @Break 50mm/min(2 inch/min) | ASTM D638 | 165 | % |
| @Yield 50mm/min(2 inch/min) | ASTM D638 | 5 | % | |
| tensile strength | @Break 50mm/min(2 inch/min) | ASTM D638 | 292 | Kgf/cm2 |
| @Yield 50mm/min(2 inch/min) | ASTM D638 | 508 | Kgf/cm2 | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Melting temperature | / | ≥196±2 | °C | |
| melt mass-flow rate | ASTM D 1238-04 | 1.8 | g/10min | |
| Hot deformation temperature | 0.45MPa | ASTM D648 | 77 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | ASTM D570 | 0.12 | % | |
| proportion | ASTM D792 | 1.29 | kg/cm3 | |
| viscosity | Ubbelodhe viscometer | 0.780±0.015 | dl/g | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dielectric loss | 1 MHz | ASTM D150 | 0.023 | – |
| 1 kHz | ASTM D150 | 0.005 | – | |
| Dielectric constant | 1 MHz | ASTM D150 | 2.4 | – |
| 1 kHz | ASTM D150 | 2.6 | – | |
| Dielectric strength | (short time,500V/sec) | ASTM D149 | 16 | kV·mm |
| Volume resistivity | ASTM D257 | 10^15 | ohm·cm | |
| Surface resistivity | ASTM D257 | 10^16 | Ohm | |
| flame retardant performance | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 1.50mm | UL 94 | HB | |
| 3.00mm | UL 94 | V-2 | ||
| 1.00mm | UL 94 | HB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.