physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ISO 1183 | 0.998 g/cm³ | |
spiral flow length | 30.0 cm |
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Shore hardness | Shore A | ISO 868 | 83 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | Break | ISO 527-2/5A/50 | 14.0 MPa |
Tensile strain | Break | ISO 527-2/5A/50 | 28 % |
elastomer | Test Condition | Test Method | Test Result |
---|---|---|---|
compression set | ISO 815 | 64 % | |
tear strength | ISO 34-1 | 63 kN/m | |
compression set | ISO 815 | 58 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.