Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
melt mass-flow rate | | ISO1133 | 3.0 g/10min |
density | | ISO1183 | 1.23 g/cm³ |
Shrinkage rate | | STM640808 | 1.1 % |
Shrinkage rate | | STM640808 | 0.57 % |
water content | | ISO960 | 0.15 % |
flammability | Test Condition | Test Method | Test Result |
---|
UL flame retardant rating | | UL94 | HB |
Hot filament ignition temperature | | IEC60695-2-13 | 650 °C |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of simply supported beam without notch | | ISO179 | 45 kJ/m² |
Impact strength of simply supported beam without notch | | ISO179 | 55 kJ/m² |
Charpy Notched Impact Strength | | ISO179 | 6.0 kJ/m² |
Charpy Notched Impact Strength | | ISO179 | 7.0 kJ/m² |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | | ISO527-2 | 5950 MPa |
Tensile stress | Yield | ISO527-2 | 110 MPa |
Tensile strain | Yield | ISO527-2 | 3.0 % |
Flexural modulus | | ISO178 | 5200 MPa |
Bending stress | | ISO178 | 172 MPa |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ISO75-2/B | 200 °C |
vicat | | ISO306/B | 200 °C |
| | ISO3146 | 220 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.