Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD792 | 1.90到2.00 g/cm³ |
Tightening rate | | ASTMD1895 | 1.0 |
Shrinkage rate | | ASTMD955 | 0.050到0.30 % |
Water absorption rate | | ASTMD570 | 0.17 % |
hardness | Test Condition | Test Method | Test Result |
---|
Barcol Hardness | | ASTMD2583 | 35到48 |
flammability | Test Condition | Test Method | Test Result |
---|
UL flame retardant rating | | UL94 | HB |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | | ASTMD638 | 34.5到41.4 MPa |
Flexural modulus | | ASTMD790 | 13800到15200 MPa |
bending strength | | ASTMD790 | 96.5到110 MPa |
Compression Modulus | | ASTMD695 | 331000到359000 MPa |
compressive strength | | ASTMD695 | 103到124 MPa |
shear strength | | ASTMD732 | 41.4到48.3 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of cantilever beam gap | | ASTMD256 | 130到190 J/m |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Inclined-PlaneTracking | | ASTMD2303 | >500 min |
dielectric strength | | ASTMD149 | 13 kV/mm |
arc resistance | | ASTMD495 | >180 sec |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTMD648 | >260 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.