Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD792 | 1.12 g/cm³ |
density | | ASTM D792 | 1.12 g/cm³ |
hardness | Test Condition | Test Method | Test Result |
---|
Shore Hardness | Shore A | ASTMD2240 | 80 |
flammability | Test Condition | Test Method | Test Result |
---|
UL flame retardant rating | | UL94 | V-0 |
Supplementary Information | Test Condition | Test Method | Test Result |
---|
OzoneResistance-Stress | | ASTMD518 | NoCracks |
Ozone Resistance - Stressed | | ASTM D518 | No Cracks |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
compression set | | ASTM D395 | 69 % |
compression set | | ASTM D395 | 49 % |
hardness | | ASTM D412 | 80 |
Tensile stress | | ASTM D412 | 3.10 MPa |
Tensile stress | | ASTM D412 | 4.30 MPa |
tensile strength | Break | ASTM D412 | 6.00 MPa |
elongation | Break | ASTM D412 | 500 % |
tear strength | | ASTM D624 | 37.0 kN/m |
compression set | | ASTM D395 | 23 % |
elastomer | Test Condition | Test Method | Test Result |
---|
Tensile stress | | ASTMD412 | 3.10 MPa |
Tensile stress | | ASTMD412 | 4.30 MPa |
tensile strength | Break | ASTMD412 | 6.00 MPa |
elongation | Break | ASTMD412 | 500 % |
tear strength | | ASTMD624 | 37.0 kN/m |
compression set | | ASTMD395 | 23 % |
compression set | | ASTMD395 | 49 % |
compression set | | ASTMD395 | 69 % |
Flame retardant performance | Test Condition | Test Method | Test Result |
---|
UL flame retardant rating | | UL 94 | V-0 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.