Basic performance | Test Condition | Test Method | Test Result |
---|---|---|---|
melt mass-flow rate | ISO 1133: Condition 4 | 0.7 g/10min | |
density | ISO 1183 | 933 kg/m | |
Carbon black content | % | IEC 811-4-1 2.6 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Environmental stress cracking resistance | ASTM D-1693 B | >1000 Hours | |
tensile strength | MPa | IEC 811-1-1 18 | |
elongation | Break | % | IEC 811-1-1 700 |
Shore hardness | ISO 868 (1Sec) | 50 |
Other performance | Test Condition | Test Method | Test Result |
---|---|---|---|
oxidation induction time | ISO TR10837 | >20 min |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
dielectric constant | IEC 250 2.5 | ||
loss factor | rad | IEC 250 3500 | |
Ω.cm | IEC 93 >10 |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
vicat | ISO 306 A | 97 ℃ | |
brittle temperature | ASTM D-746 | <-100 ℃ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.