physical property Test ConditionTest MethodTest Result
densityASTM D15050.910 g/cm³
melt mass-flow rateASTM D12383.0 g/10min
flammabilityTest ConditionTest MethodTest Result
UL flame retardant ratingUL 94HB
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTM D25625 J/m
Impact strength of cantilever beam gapASTM D25639 J/m
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strength YieldASTM D63837.3 MPa
tensile strength BreakASTM D63834.3 MPa
elongationBreakASTM D638500 %
Thermal performanceTest ConditionTest MethodTest Result
Hot deformation temperature (HDT)ASTM D648110 °C
Hot deformation temperature (HDT)ASTM D64860.0 °C
vicatASTM D1525155 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.