Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
AcidValue | | | 15.00到20.00 mgKOH/g |
StyreneContent | | | 35到38 % |
Uncured Properties | Test Condition | Test Method | Test Result |
---|
| | | 0.45到0.68 Pa·s |
Curing Time | | | 0.42到0.62 hr |
GelTime | | | 14到22 min |
density | | | 1.12 g/cm³ |
Supplementary Information | Test Condition | Test Method | Test Result |
---|
PeakExotherm | | | 175到186 °C |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | | | 4100 MPa |
Tensile stress | | | 86.0 MPa |
Tensile strain | Break | | 4.4 % |
Flexural modulus | | | 4250 MPa |
Bending stress | | | 165 MPa |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | | 80 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.