Copolyester 90

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTMD7921.28 g/cm³
optical performance Test ConditionTest MethodTest Result
transmissivityASTMD100391.0 %
Haze ratioASTMD10031.0 %
Mechanical propertiesTest ConditionTest MethodTest Result
elongationBreakASTMD638220 %
Flexural modulusASTMD7902500 MPa
bending strengthYieldASTMD79089.0 MPa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTMD25625 J/m
Thermal performanceTest ConditionTest MethodTest Result
Glass Transition TemperatureASTMD742695.0 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.

Contact Us

Get App

Top