Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
melt mass-flow rate | | ASTM D1238 | 11 g/10 min |
Shrinkage rate | | ASTM D955 | 0.50 - 0.80 % |
Outdoor applicability | | UL 746C | f1 |
hardness | Test Condition | Test Method | Test Result |
---|
Rockwell hardness | | ASTM D785 | 118 |
optical performance | Test Condition | Test Method | Test Result |
---|
transmissivity | | JIS K7361 | 80.0 % |
flammability | Test Condition | Test Method | Test Result |
---|
UL flame retardant rating | | UL 94 | V-2 |
UL flame retardant rating | | UL 94 | V-2 |
UL flame retardant rating | | UL 94 | V-2 |
UL flame retardant rating | | UL 94 | V-2 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | | ASTM D638 | 61.8 Mpa |
elongation | | ASTM D638 | > 100 % |
Flexural modulus | | ASTM D790 | 2260 Mpa |
bending strength | | ASTM D790 | 93.2 Mpa |
squeeze out | Test Condition | Test Method | Test Result |
---|
drying temperature | | | 100 to 120 °C |
drying time | | | 3.0 to 4.0 hr |
Suggested maximum moisture content | | | 0.020 % |
Temperature in Zone 1 of the material cylinder | | | 260 to 280 °C |
Temperature in Zone 2 of the material cylinder | | | 270 to 300 °C |
Temperature in Zone 3 of the material cylinder | | | 270 to 300 °C |
Temperature in Zone 4 of the material cylinder | | | 270 to 300 °C |
Joint temperature | | | 280 to 300 °C |
Melt Temperature | | | 300 to 320 °C |
die temperature | | | 260 to 295 °C |
injection | Test Condition | Test Method | Test Result |
---|
drying temperature | | | 100 to 120 °C |
drying time | | | 3.0 to 4.0 hr |
Suggested maximum moisture content | | | 0.020 % |
Temperature at the rear of the barrel | | | 260 to 280 °C |
Temperature in the middle of the barrel | | | 280 to 300 °C |
Temperature at the front of the material cylinder | | | 290 to 310 °C |
Spray nozzle temperature | | | 290 to 310 °C |
Processing (melt) temperature | | | 300 to 320 °C |
Temperature | | | 80 to 120 °C |
Back pressure | | | 0.981 to 3.92 Mpa |
screw speed | | | 40 to 70 rpm |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Heat distortion temperature | | ASTM D648 | 130 °C |
RTI Elec | | UL 746 | 120 °C |
RTI Imp | | UL 746 | 105 °C |
RTI | | UL 746 | 120 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.