| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 37 | kJ/m² |
| -30°C | ISO 179/1eU | 26 | kJ/m² | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 1.5mm | UL 94 | HB | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| bending strength | 23°C | ISO 178 | 111 | MPa |
| Bending modulus | 23°C | ISO 178 | 4150 | MPa |
| Tensile strain | Break,23°C | ISO 527-2/5 | 7.0 | % |
| tensile strength | 23°C | ISO 527-2/5 | 78.0 | MPa |
| Tensile modulus | 23°C | ISO 527-2/1 | 4250 | MPa |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Vicat softening temperature | ISO 306/B50 | 125 | °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 108 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Shrinkage rate | TD:23°C,3.00mm | ISO 294-4 | 0.60 | % |
| Water absorption rate | 23°C,24hr | ISO 62 | 0.20 | % |
| Shrinkage rate | MD:23°C,3.00mm | ISO 294-4 | 0.20 | % |
| melt mass-flow rate | 260°C/5.0kg | ISO 1133 | 25 | g/10min |
| density | 23°C | ISO 1183 | 1.22 | g/cm³ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.