physical property Test ConditionTest MethodTest Result
densityASTM D7921.24 g/cm³
melt mass-flow rateASTM D12388.0to12 g/10min
Shrinkage rateASTM D9550.80 %
hardnessTest ConditionTest MethodTest Result
Hardness (Shore)ASTM D141577
Mechanical propertiesTest ConditionTest MethodTest Result
bending strengthASTM D79055.2 MPa
Tensile modulusASTM D6382620 MPa
tensile strength ASTM D63831.7 MPa
elongationASTM D6383.5 %
elongationASTM D63810 %
Flexural modulusASTM D7902760 MPa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTM D25627 J/m
GardnerImpactASTM D30290.565 J
Thermal performanceTest ConditionTest MethodTest Result
Hot deformation temperature (HDT)ASTM D648138 °C
Hot deformation temperature (HDT)ASTM D64879.4 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.