Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | | 1.41 g/cm³ |
Shrinkage rate | | | 1.1to1.3 % |
Shrinkage rate | | | 0.60to0.80 % |
Shrinkage rate | | | 0.90to1.1 % |
Shrinkage rate | | | <0.40 % |
flammability | Test Condition | Test Method | Test Result |
---|
UL flame retardant rating | | UL 94 | V-0 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
bending strength | | | 88.0to118 MPa |
compressive strength | | | 225to255 MPa |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Compared to the Leakage Tracking Index (CTI) | | | PLC 4 |
insulation resistance | | | 1.0E+8到1.0E+9 ohms |
insulation resistance | | | 1.0E+9到1.0E+10 ohms |
dielectric strength | | | >8.0 kV/mm |
arc resistance | | | 140 sec |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Heat distortion temperature | | | 170 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.