Share
Add to Compare

PBT Generic ABS+PBT - Glass Fiber Generic

Properties:
Filler glass fiber reinforced material
Product Description
Certificates(0)
Datasheet

Product Description

Properties:Filler | glass fiber reinforced material

Certificates

No Data...

Technical Data Sheet

impact performanceTest ConditionTest MethodTest ResultTest Unit
Charpy Notched Impact Strength23°CISO 1795.9to8.2kJ/m²
Impact strength of cantilever beam gap23°CASTM D25656to83J/m
mechanical propertiesTest ConditionTest MethodTest ResultTest Unit
elongationBreak,23°CISO 527-22.5to3.5%
tensile strengthYield,23°CASTM D63867.1to123MPa
tensile strengthYield,23°CISO 527-278.8to120MPa
tensile strengthBreak,23°CASTM D63877.5to112MPa
Bending modulus23°CASTM D7903180to10300MPa
Bending modulus23°CISO 1783800to9770MPa
bending strength23°CASTM D79086.1to190MPa
bending strength23°CISO 178114to171MPa
tensile strength23°CASTM D63877.7to105MPa
elongationBreak,23°CASTM D6381.5to4.4%
thermal performanceTest ConditionTest MethodTest ResultTest Unit
Hot deformation temperature0.45MPa,UnannealedISO 75-2/B196to220°C
Hot deformation temperature1.8MPa,UnannealedASTM D648104to202°C
Hot deformation temperature1.8MPa,UnannealedISO 75-2/A104to191°C
Vicat softening temperatureISO 306100to218°C
Linear coefficient of thermal expansionMDASTM D6962.8E-5到6.6E-5cm/cm/°C
Linear coefficient of thermal expansionMDISO 11359-22.0E-5到4.0E-5cm/cm/°C
Hot deformation temperature0.45MPa,UnannealedASTM D648198to211°C
Linear coefficient of thermal expansionTDISO 11359-27.9E-5到1.0E-4cm/cm/°C
RTI ElecUL 74659.0to140°C
RTI ImpUL 74658.8to100°C
RTIUL 74660.0to130°C
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
density23°CISO 11831.28to1.61g/cm³
melt mass-flow rate250°C/5.0kgASTM D123814to40g/10min
Shrinkage rateMD:23°CASTM D9550.20to0.67%
Water absorption rate23°C,24hrASTM D5700.12to0.15%
Water absorption rate23°C,24hrISO 620.15%
density--ASTM D7921.23to1.55g/cm³
Electrical performanceTest ConditionTest MethodTest ResultTest Unit
Volume resistivity23°CASTM D2571.0E+15到1.0E+17ohms·cm
Volume resistivity23°CIEC 600931.0E+15到2.5E+17ohms·cm
Dielectric strength23°CASTM D14918to35kV/mm
Arc resistanceASTM D49569.0to85.5sec
Compared to the anti leakage trace indexIEC 60112PLC 0
High arc combustion indexHAIUL 746PLC 1
High voltage arc tracing rateHVTRUL 746PLC 4mm/min
Hot wire ignitionHWIUL 746PLC 2sec
hardnessTest ConditionTest MethodTest ResultTest Unit
Rockwell hardness23°CASTM D785114to120
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.